Rapid strength gain concrete for floor toppings and repair

Description

Ronaset Concrete is supplied as a pre-packed, two component, ready to use mortar. It is supplied complete with all the dry components in a bag and a bottle of gauging liquid. Ronaset Concrete’s rapid strength gain is used for laying new and repairing existing floors and bedding building components.

 

Surfaces formed using Ronaset Concrete can be trafficked as early as 18 – 24 hours after mixing. The speed of Ronaset Concrete makes it ideal for application in areas where surfaces must be formed or reinstated or components bedded and opened to traffic with minimum disruption and delay.

 

As well as offering rapid strength gain Ronaset Concrete is strong and durable and capable of achieving 28 day strengths of conventional mortar within hours. Its formulation also allows it to be applied at minimum temperatures of 0°C facilitating external work during cold weather and in cold stores.

Applications for Ronaset Concrete include:
• high strength industrial toppings
• high abrasion resistant floors
• thick section patch repairs in high demand/constant access areas

 

Ronaset Concete Technical Data

Coverage per pack0.42m² @ 25mm
0.21m² @ 50mm
0.14m² @ 75mm
0.10m² @ 100mm
Yield per pack10.5 litres
Packs required per m³95 packs (approx)
Minimum thickness25mm
Maximum thickness100mm per lyaer
Compressive Strength (24 hours)40N/mm²
Compressive Strength (7 days)52N/mm²
Compressive Strength (28 days)60N/mm²

    Quick Question?







    Our Product range

    RonaScreed FastDry Prompt – benefits and drying

    RonaScreed FastDry Prompt (formerly RonaScreed 8 Day Overlay) is so-called because it is a fast-drying screed additive which enables a 50mm thickness of 3:1 sand/ cement screed to be overlaid with moi ...

    Read more

    Drying of Screeds

    BS 8204-1 “Concrete bases and cementitious levelling screeds to receive floorings — Code of practice” section 6.11.1 suggests the following calculation for drying of screeds with no fast drying additi ...

    Read more

    Avoidance/ Mitigation Of The Effects Of Common Forms Of Cracking In Cementitious Screeds

    Aggregate is usually 0–4 mm and is mixed with cement in the ratio of 1:3 or 1:4 cement to sand, depending on strength requirements and drying requirements. For total screed thicknesses in excess of 50 ...